since early 2010 we have been testing our products in real-life circumstances. after 25 pours with plicafix repaired plywood formwork, the repair spots are still looking and working very good.
this is the setup:
- pouring with fairface concrete (small grains 0-16mm additives)
- 72 hrs in formwork
- formwork cleaning with brush, water
- oiling
- next pour
see the image below
the plicafix plywood repair spot is barely visible just right and below the center of the board. the damage on top left is growing with every pour. we left the damage to show the difference between repaired and unrepaired form.
No comments:
Post a Comment